{"id":6958,"date":"2025-07-15T13:32:24","date_gmt":"2025-07-15T05:32:24","guid":{"rendered":"https:\/\/www.qualitester.com\/?page_id=6958"},"modified":"2025-07-15T13:32:24","modified_gmt":"2025-07-15T05:32:24","slug":"finat-ftm-9","status":"publish","type":"page","link":"https:\/\/www.qualitester.com\/pt\/standards\/finat-ftm-9\/","title":{"rendered":"FINAT FTM 9"},"content":{"rendered":"<h1 style=\"text-align: center;\" data-start=\"370\" data-end=\"882\">FINAT FTM 9<br \/>\n<small>Ensaio de ader\u00eancia do la\u00e7o<\/small><\/h1>\n<hr \/>\n<p data-start=\"437\" data-end=\"768\">Os adesivos sens\u00edveis \u00e0 press\u00e3o (PSA) s\u00e3o essenciais na embalagem, rotulagem e outras aplica\u00e7\u00f5es industriais, onde a sua <strong data-start=\"558\" data-end=\"574\">tacha inicial<\/strong>-A capacidade de agarrar rapidamente uma superf\u00edcie \u00e9 fundamental. A <strong data-start=\"630\" data-end=\"645\">FINAT FTM 9<\/strong> O m\u00e9todo de ensaio fornece um procedimento fi\u00e1vel e normalizado para medir esta propriedade atrav\u00e9s de uma configura\u00e7\u00e3o de ader\u00eancia em la\u00e7o.<\/p>\n<p data-start=\"770\" data-end=\"1180\">Utilizado globalmente no controlo de qualidade e I&amp;D, <em data-start=\"812\" data-end=\"825\">FINAT FTM 9<\/em> desempenha um papel crucial na ajuda aos fabricantes na sele\u00e7\u00e3o dos materiais adesivos mais eficazes, particularmente para linhas de etiquetagem autom\u00e1tica de alta velocidade. Neste artigo, iremos aprofundar os <strong data-start=\"1012\" data-end=\"1037\">m\u00e9todo de ensaio de ader\u00eancia em anel<\/strong>, A Cell Instruments\u2019 \u00e9 uma empresa de consultoria que se dedica \u00e0 investiga\u00e7\u00e3o e desenvolvimento de produtos e servi\u00e7os, \u00e0 sua import\u00e2ncia, aos procedimentos, aos requisitos de equipamento e \u00e0 forma como a Cell Instruments' <em data-start=\"1117\" data-end=\"1142\"><a href=\"https:\/\/www.qualitester.com\/pt\/produto\/sale-tape-loop-tack-testing-machine\/\">LTT-01<\/a> Testador de ader\u00eancia de loop<\/em> garante o cumprimento da norma.<\/p>\n<hr \/>\n<h2 data-start=\"770\" data-end=\"1180\">O que \u00e9 o FINAT FTM 9?<\/h2>\n<p data-start=\"1213\" data-end=\"1568\"><strong data-start=\"1213\" data-end=\"1228\">FINAT FTM 9<\/strong> \u00e9 um m\u00e9todo de ensaio normalizado publicado pela FINAT (a associa\u00e7\u00e3o europeia para a ind\u00fastria de etiquetas auto-adesivas) para determinar a <strong data-start=\"1362\" data-end=\"1375\">prego de la\u00e7o<\/strong> de materiais sens\u00edveis \u00e0 press\u00e3o. A ader\u00eancia, distinta da ades\u00e3o ou coes\u00e3o, refere-se \u00e0 capacidade do adesivo para formar uma liga\u00e7\u00e3o imediata com um substrato sob um breve contacto e uma press\u00e3o m\u00ednima.<\/p>\n<p data-start=\"1570\" data-end=\"1779\">Este m\u00e9todo oferece uma forma pr\u00e1tica de comparar a for\u00e7a de \u201cagarramento\u201d de diferentes materiais de etiquetas ou fitas, uma propriedade que \u00e9 especialmente relevante em ambientes de aplica\u00e7\u00e3o r\u00e1pida, tais como m\u00e1quinas de etiquetagem.<\/p>\n<hr \/>\n<h2 data-start=\"1570\" data-end=\"1779\">Porque \u00e9 que o teste do la\u00e7o \u00e9 importante?<\/h2>\n<p data-start=\"1827\" data-end=\"2059\">O <strong data-start=\"1831\" data-end=\"1844\">prego de la\u00e7o<\/strong> est\u00e1 diretamente relacionado com o desempenho da aplica\u00e7\u00e3o, especialmente em sistemas em que a cola deve aderir instantaneamente com um tempo de perman\u00eancia m\u00ednimo. Um valor elevado de \"loop tack\" indica uma melhor ader\u00eancia imediata, cr\u00edtica em:<\/p>\n<ul>\n<li data-start=\"2063\" data-end=\"2120\"><strong data-start=\"2063\" data-end=\"2084\">M\u00e1quinas de etiquetagem<\/strong> onde os materiais devem aderir instantaneamente<\/li>\n<li data-start=\"2123\" data-end=\"2152\"><strong data-start=\"2123\" data-end=\"2152\">Aplica\u00e7\u00f5es de fitas m\u00e9dicas<\/strong><\/li>\n<li data-start=\"2155\" data-end=\"2203\"><strong data-start=\"2155\" data-end=\"2177\">Embalagens de consumo<\/strong> que requerem um encerramento imediato<\/li>\n<li data-start=\"2206\" data-end=\"2233\"><strong data-start=\"2206\" data-end=\"2233\">Necessidades tempor\u00e1rias de colagem<\/strong><\/li>\n<\/ul>\n<p data-start=\"2235\" data-end=\"2373\">A medi\u00e7\u00e3o exacta da ader\u00eancia do la\u00e7o ajuda os fabricantes a controlar a qualidade, a afinar as formula\u00e7\u00f5es e a satisfazer as expectativas de desempenho dos clientes.<\/p>\n<hr \/>\n<h2 data-start=\"2235\" data-end=\"2373\">Vis\u00e3o geral do m\u00e9todo de teste Loop Tack<\/h2>\n<p>O <strong data-start=\"2420\" data-end=\"2445\">m\u00e9todo de ensaio de ader\u00eancia em anel<\/strong>, tal como definido em <em data-start=\"2461\" data-end=\"2474\">FINAT FTM 9<\/em>, O m\u00e9todo de medi\u00e7\u00e3o da for\u00e7a de descolamento, que consiste em colocar uma tira de material sens\u00edvel \u00e0 press\u00e3o em contacto com um substrato normalizado (normalmente vidro flotado) e depois separ\u00e1-la a uma velocidade fixa para medir a for\u00e7a m\u00e1xima de descolamento.<\/p>\n<h3>Equipamento de teste<\/h3>\n<ul>\n<li data-start=\"2704\" data-end=\"2892\">UM <strong data-start=\"2706\" data-end=\"2724\">testador de tra\u00e7\u00e3o<\/strong> ou m\u00e1quina de ensaio universal com uma velocidade de separa\u00e7\u00e3o das maxilas verticais de <strong data-start=\"2794\" data-end=\"2808\">300 mm\/min<\/strong>, dire\u00e7\u00e3o revers\u00edvel, e medi\u00e7\u00e3o de for\u00e7a at\u00e9 <strong data-start=\"2860\" data-end=\"2873\">20 Newton<\/strong> com uma exatid\u00e3o de \u00b12%.<\/li>\n<li data-start=\"2895\" data-end=\"2984\">UM <strong data-start=\"2897\" data-end=\"2912\">placa de vidro<\/strong> de 25 mm \u00d7 30 mm (\u00b1 toler\u00e2ncias), fixada a uma cavilha para montagem.<\/li>\n<\/ul>\n<hr \/>\n<h2>Prepara\u00e7\u00e3o e condicionamento de amostras<\/h2>\n<ul>\n<li data-start=\"3211\" data-end=\"3272\">As tiras devem ser <strong data-start=\"3228\" data-end=\"3258\">25 mm de largura e 175 mm de comprimento<\/strong>, bem cortado.<\/li>\n<li data-start=\"3275\" data-end=\"3323\">O material de suporte \u00e9 removido imediatamente antes do ensaio.<\/li>\n<li data-start=\"3326\" data-end=\"3411\">As tiras s\u00e3o enroladas com <strong data-start=\"3349\" data-end=\"3370\">lado adesivo para fora<\/strong> e fixada no maxilar superior do aparelho de controlo.<\/li>\n<li data-start=\"3414\" data-end=\"3560\">As condi\u00e7\u00f5es de teste s\u00e3o definidas em <strong data-start=\"3441\" data-end=\"3455\">23\u00b0C \u00b1 2\u00b0C<\/strong> e <strong data-start=\"3460\" data-end=\"3475\">50% RH \u00b1 5%<\/strong> com um m\u00ednimo de <strong data-start=\"3491\" data-end=\"3514\">Condicionamento de 4 horas<\/strong> para os provetes e para o substrato.<\/li>\n<\/ul>\n<hr \/>\n<h2>Procedimento de ensaio<\/h2>\n<ol>\n<li data-start=\"3590\" data-end=\"3648\">Enrole a fita adesiva e insira-a no punho superior.<\/li>\n<li data-start=\"3652\" data-end=\"3702\">Fixar a placa de vidro limpa no punho inferior.<\/li>\n<li data-start=\"3706\" data-end=\"3780\">Colocar o la\u00e7o de cola em contacto com o substrato em <strong data-start=\"3765\" data-end=\"3779\">300 mm\/min<\/strong>.<\/li>\n<li data-start=\"3784\" data-end=\"3853\">Inverta imediatamente a dire\u00e7\u00e3o para separar o circuito \u00e0 mesma velocidade.<\/li>\n<li data-start=\"3857\" data-end=\"3916\">Registar o <strong data-start=\"3868\" data-end=\"3882\">for\u00e7a m\u00e1xima<\/strong> (excluindo os picos de ru\u00eddo iniciais).<\/li>\n<li data-start=\"3920\" data-end=\"3993\">Repetir com <strong data-start=\"3932\" data-end=\"3948\">cinco amostras<\/strong> e comunicar o valor m\u00e9dio em <strong data-start=\"3981\" data-end=\"3992\">Novotons<\/strong>.<\/li>\n<\/ol>\n<p data-start=\"3995\" data-end=\"4005\">Nota\u00e7\u00f5es:<\/p>\n<ul>\n<li data-start=\"4008\" data-end=\"4080\">Se o rasg\u00e3o ocorrer antes da liberta\u00e7\u00e3o do adesivo \u2192 marcar com <em data-start=\"4062\" data-end=\"4066\">PT<\/em> (rasg\u00e3o no papel).<\/li>\n<li data-start=\"4083\" data-end=\"4186\">Se a cola se transferir para a placa \u2192 marcar com <em data-start=\"4130\" data-end=\"4134\">AT<\/em> (transfer\u00eancia de adesivo), com indica\u00e7\u00e3o da percentagem aproximada.\n<div class=\"ast-oembed-container\" style=\"height: 100%;\"><iframe title=\"Amostra de teste do Finat 9 Loop Tack\" width=\"500\" height=\"281\" src=\"https:\/\/www.youtube.com\/embed\/tVZSoEi7Blk?feature=oembed\" frameborder=\"0\" allow=\"accelerometer; autoplay; clipboard-write; encrypted-media; gyroscope; picture-in-picture; web-share\" referrerpolicy=\"strict-origin-when-cross-origin\" allowfullscreen><\/iframe><\/div>\n<\/li>\n<\/ul>\n<hr \/>\n<h2>Factores que influenciam a precis\u00e3o do teste<\/h2>\n<p data-start=\"4232\" data-end=\"4279\">Existem diversas vari\u00e1veis que podem afetar os resultados da ader\u00eancia do la\u00e7o:<\/p>\n<ul>\n<li data-start=\"4283\" data-end=\"4446\"><strong data-start=\"4283\" data-end=\"4308\">Limpeza do substrato<\/strong> - Utilizar solventes n\u00e3o residuais como MEK, acetona ou n-heptano. Repetir a limpeza tr\u00eas vezes e deixar as placas em repouso durante 4 horas antes de as utilizar.<\/li>\n<li data-start=\"4449\" data-end=\"4507\"><strong data-start=\"4449\" data-end=\"4468\">Rigidez da amostra<\/strong> - Afecta a forma do la\u00e7o e a \u00e1rea de contacto.<\/li>\n<li data-start=\"4510\" data-end=\"4618\"><strong data-start=\"4510\" data-end=\"4538\">Condi\u00e7\u00f5es ambientais<\/strong> - Deve ser rigorosamente controlado, uma vez que a ader\u00eancia \u00e9 sens\u00edvel \u00e0 humidade e \u00e0 temperatura.<\/li>\n<\/ul>\n<hr \/>\n<h2>Porqu\u00ea escolher <a href=\"https:\/\/www.qualitester.com\/pt\/\">Instrumentos de C\u00e9lula<\/a>\u2019 LTT-01 para teste de ader\u00eancia do la\u00e7o<\/h2>\n<figure id=\"attachment_6966\" aria-describedby=\"caption-attachment-6966\" style=\"width: 300px\" class=\"wp-caption alignright\"><a href=\"https:\/\/www.qualitester.com\/pt\/produto\/sale-tape-loop-tack-testing-machine\/\"><img fetchpriority=\"high\" decoding=\"async\" class=\"wp-image-6966 size-medium\" src=\"https:\/\/www.qualitester.com\/wp-content\/uploads\/2025\/07\/Tape-Loop-Tack-Testing-Machine-300x300.webp\" alt=\"O FINAT FTM 9 \u00e9 um m\u00e9todo normalizado de ensaio de ader\u00eancia de la\u00e7os.\" width=\"300\" height=\"300\" srcset=\"https:\/\/www.qualitester.com\/wp-content\/uploads\/2025\/07\/Tape-Loop-Tack-Testing-Machine-300x300.webp 300w, https:\/\/www.qualitester.com\/wp-content\/uploads\/2025\/07\/Tape-Loop-Tack-Testing-Machine-150x150.webp 150w, https:\/\/www.qualitester.com\/wp-content\/uploads\/2025\/07\/Tape-Loop-Tack-Testing-Machine-12x12.webp 12w, https:\/\/www.qualitester.com\/wp-content\/uploads\/2025\/07\/Tape-Loop-Tack-Testing-Machine-100x100.webp 100w, https:\/\/www.qualitester.com\/wp-content\/uploads\/2025\/07\/Tape-Loop-Tack-Testing-Machine.webp 600w\" sizes=\"(max-width: 300px) 100vw, 300px\" \/><\/a><figcaption id=\"caption-attachment-6966\" class=\"wp-caption-text\">Testador de ader\u00eancia de loop LTT-01<\/figcaption><\/figure>\n<p data-start=\"4688\" data-end=\"4809\">O <strong data-start=\"4692\" data-end=\"4719\">Testador de ader\u00eancia de loop LTT-01<\/strong> da Cell Instruments foi concebido especificamente para satisfazer <strong data-start=\"4775\" data-end=\"4790\">FINAT FTM 9<\/strong> requisitos com:<\/p>\n<ul>\n<li data-start=\"4813\" data-end=\"4887\"><strong data-start=\"4813\" data-end=\"4836\">Mec\u00e2nica de precis\u00e3o<\/strong> assegurando um contacto\/separa\u00e7\u00e3o constante de 300 mm\/min.<\/li>\n<li data-start=\"4890\" data-end=\"4964\"><strong data-start=\"4890\" data-end=\"4945\">Controlo por ecr\u00e3 t\u00e1til e sequ\u00eancias de teste program\u00e1veis<\/strong> para a repetibilidade.<\/li>\n<li data-start=\"4967\" data-end=\"5042\"><strong data-start=\"4967\" data-end=\"4993\">Sa\u00edda de dados em Newtons<\/strong>, incluindo o c\u00e1lculo autom\u00e1tico da m\u00e9dia de v\u00e1rias execu\u00e7\u00f5es.<\/li>\n<li data-start=\"5045\" data-end=\"5099\"><strong data-start=\"5045\" data-end=\"5081\">Conformidade com as normas mundiais<\/strong> para o ensaio de ader\u00eancia.<\/li>\n<\/ul>\n<p data-start=\"5101\" data-end=\"5318\">Para os fabricantes e laborat\u00f3rios que pretendem garantir uma qualidade consistente do produto ou cumprir os padr\u00f5es de desempenho de adesivos espec\u00edficos do cliente e regulamentares, o LTT-01 oferece o equil\u00edbrio ideal entre precis\u00e3o, facilidade de utiliza\u00e7\u00e3o e fiabilidade.<\/p>\n<hr \/>\n<h2 data-start=\"5101\" data-end=\"5318\">Conclus\u00e3o<\/h2>\n<p data-start=\"5341\" data-end=\"5700\">O <strong data-start=\"5345\" data-end=\"5360\">FINAT FTM 9<\/strong> O m\u00e9todo de ensaio de ader\u00eancia em anel \u00e9 uma ferramenta essencial para avaliar a ader\u00eancia inicial das colas sens\u00edveis \u00e0 press\u00e3o. Ao adotar esta abordagem normalizada e ao utilizar instrumentos fi\u00e1veis como o <strong data-start=\"5546\" data-end=\"5573\">Testador de ader\u00eancia de loop LTT-01<\/strong> de <strong data-start=\"5579\" data-end=\"5599\">Instrumentos de C\u00e9lula<\/strong>, Com esta tecnologia, os fabricantes podem assegurar uma colagem de elevado desempenho em aplica\u00e7\u00f5es de etiquetagem, embalagem e m\u00e9dicas.<\/p>\n<p data-start=\"5702\" data-end=\"5854\">Compreender os valores de ader\u00eancia do loop n\u00e3o se trata apenas de n\u00fameros - trata-se de otimizar o desempenho, reduzir as taxas de falha e melhorar a satisfa\u00e7\u00e3o do utilizador final.<\/p>","protected":false},"excerpt":{"rendered":"<p>FINAT FTM 9 Loop Tack Testing Os adesivos sens\u00edveis \u00e0 press\u00e3o (PSAs) s\u00e3o essenciais em embalagens, etiquetas e outras aplica\u00e7\u00f5es industriais, onde a sua ader\u00eancia inicial - a capacidade de agarrar rapidamente uma superf\u00edcie - \u00e9 cr\u00edtica. O m\u00e9todo de ensaio FINAT FTM 9 fornece um procedimento fi\u00e1vel e normalizado para medir esta propriedade atrav\u00e9s de uma configura\u00e7\u00e3o de ader\u00eancia em loop. Utilizado globalmente no controlo de qualidade ...<\/p>\n<p class=\"read-more\"> <a class=\"\" href=\"https:\/\/www.qualitester.com\/pt\/standards\/finat-ftm-9\/\"> <span class=\"screen-reader-text\">FINAT FTM 9<\/span> Ler mais \"<\/a><\/p>","protected":false},"author":3,"featured_media":0,"parent":4948,"menu_order":0,"comment_status":"closed","ping_status":"closed","template":"","meta":{"site-sidebar-layout":"default","site-content-layout":"default","ast-global-header-display":"","ast-main-header-display":"","ast-hfb-above-header-display":"","ast-hfb-below-header-display":"","ast-hfb-mobile-header-display":"","site-post-title":"","ast-breadcrumbs-content":"","ast-featured-img":"","footer-sml-layout":"","theme-transparent-header-meta":"default","adv-header-id-meta":"","stick-header-meta":"","header-above-stick-meta":"","header-main-stick-meta":"","header-below-stick-meta":"","footnotes":""},"class_list":["post-6958","page","type-page","status-publish","hentry"],"_links":{"self":[{"href":"https:\/\/www.qualitester.com\/pt\/wp-json\/wp\/v2\/pages\/6958","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/www.qualitester.com\/pt\/wp-json\/wp\/v2\/pages"}],"about":[{"href":"https:\/\/www.qualitester.com\/pt\/wp-json\/wp\/v2\/types\/page"}],"author":[{"embeddable":true,"href":"https:\/\/www.qualitester.com\/pt\/wp-json\/wp\/v2\/users\/3"}],"replies":[{"embeddable":true,"href":"https:\/\/www.qualitester.com\/pt\/wp-json\/wp\/v2\/comments?post=6958"}],"version-history":[{"count":0,"href":"https:\/\/www.qualitester.com\/pt\/wp-json\/wp\/v2\/pages\/6958\/revisions"}],"up":[{"embeddable":true,"href":"https:\/\/www.qualitester.com\/pt\/wp-json\/wp\/v2\/pages\/4948"}],"wp:attachment":[{"href":"https:\/\/www.qualitester.com\/pt\/wp-json\/wp\/v2\/media?parent=6958"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}